dc.descriptionThe heterogeneous photocatalytic degradation of dyes reactive red 120 and reactive blue 4 under ideal solutions and hydrolysates dyes simulating a staining process with an initial concentration of 50 mg • L-1 was studied, using 200 mg • L-1 of TiO2 doped with Fe or N. Total degradation of both dyes was achieved with the addition of an auxiliary oxidizing agent such as hydrogen peroxide (H2O2) at a concentration of 12.0 mM. Such degradation was achieved after one hour of reaction for doped catalysts (N-TiO2 and Fe-TiO2). For solutions of hydrolysed dye that simulated waste water from the textile industry was found that the pH adversely affects dye degradation due to repulsion between the photocatalysts and dyes. In all the studied cases further degradation of reactive red dye 120 was observed relative to reactive blue 4, which can be associated with the complex molecular structure of the second dye.en-US
dc.descriptionSe estudió la degradación fotocatalítica heterogénea de los colorantes rojo reactivo 120 y azul reactivo 4 en soluciones ideales y colorantes hidrolizados simulando un proceso de tinción con una concentración inicial de 50 mg·L-1, usando 200 mg·L-1 de TiO2 dopado con Fe o N. Se logró la degradación total de ambos colorantes con la adición de un agente oxidante auxiliar como el peróxido de hidrógeno (H2O2) en una concentración de 12.0 mM. Dicha degradación se logró luego de una hora de reacción para los catalizadores dopados (N-TiO2 y Fe-TiO2), sin embargo, para las soluciones de colorante hidrolizado que simularon un agua residual de la industria textil se encontró que el pH afecta negativamente la degradación de los colorantes debido a la repulsión ocasionada entre los fotocatalizadores y los colorantes. En todos los casos estudiados se observó una mayor degradación del colorante rojo reactivo 120 respecto al azul reactivo 4, lo cual se puede deber a la compleja estructura molecular del segundo colorante.es-ES
dc.formatapplication/pdf
dc.identifierhttps://revistas.elpoli.edu.co/index.php/pol/article/view/483
dc.identifier.urihttps://repositorio.elpoli.edu.co/handle/123456789/929
dc.languagespa
dc.publisherPolitécnico Colombiano Jaime Isaza Cadavides-ES
dc.relationhttps://revistas.elpoli.edu.co/index.php/pol/article/view/483/510
dc.sourceRevista Politécnica; Vol. 11 No. 20: January-June; 9-19en-US
dc.sourceRevista Politécnica; Vol. 11 Núm. 20: Enero-Junio, 2015; 9-19es-ES
dc.sourceRevista Politécnica; v. 11 n. 20: Enero-Junio, 2015; 9-19pt-BR
dc.source2256-5353
dc.source1900-2351
dc.subjectPhotocatalytic degradationen-US
dc.subjectreactive red 120en-US
dc.subjectreactive blue 4en-US
dc.subjectTiO2en-US
dc.subjectN-TiO2en-US
dc.subjectFe-TiO2en-US
dc.subjectDegradación fotocatalíticaes-ES
dc.subjectcolorante rojo reactivo 120es-ES
dc.subjectcolorante azul reactivo 4es-ES
dc.subjectTiO2es-ES
dc.subjectH2O2es-ES
dc.subjectcatalizadores dopadoses-ES
dc.subjectN-TiO2es-ES
dc.subjectFe-TiO2es-ES
dc.subjectDegradación químicaes-ES
dc.subjectColorantes reactivoses-ES
dc.subjectCatalizadores.es-ES
dc.titlePhotocatalytic degradation of hydrolyzed reactive red 120 and reactive blue 4 using nitrogen or iron doped tio2en-US
dc.titleDegradación fotocatalítica de los colorantes rojo reactivo 120 y azul reactivo 4 hidrolizados usando tio2 dopado con hierro o nitrógenoes-ES
dc.typeinfo:eu-repo/semantics/article
dc.typeinfo:eu-repo/semantics/publishedVersion
Files